Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature -30.0 °C |
7.00 ft-lb/in @Temperature -22.0 °F |
0.125in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | ASTM D256 |
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | |
MTI ThermoStran® PA66-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature -30.0 °C |
7.00 ft-lb/in @Temperature -22.0 °F |
0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | -22°F; ASTM D256 |
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
Aclo Accucomp ABS ABS811L Medium Impact Grade |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D628 |
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast.. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Izod Impact, Notched | 3.74 - 5340 J/cm | 7.00 - 10000 ft-lb/in | Average value: 4.50 J/cm Grade Count:9 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D628 |
ACC EP QS EPI Engineered Polymers Quick Set Epoxy EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |