Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.47 J/cm @Temperature 23.0 °C |
6.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 50% long glass fiber reinforcementInformation provided by PlastiC.. |
|||
Izod Impact, Notched | 3.47 J/cm @Temperature 23.0 °C |
6.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG37CR ABS High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 3.47 J/cm @Temperature 23.0 °C |
6.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific) High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MGABS01 ABS Injection molding ABS. High impact, high gloss, good flow. |
|||
Izod Impact, Notched | 3.47 J/cm @Temperature -30.0 °C |
6.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | Method A; ASTM D256 |
Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer COPYLENE® CR020CL is a random copolymer formulated with advanced clarifier technology and with antistat and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have .. |
|||
Izod Impact, Notched | 3.47 J/cm @Temperature -30.0 °C |
6.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific) Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Izod Impact, Notched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ASA 814 GY Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PN235 PPE+PS Plating grade, primarily automotive applications. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PN235 PPE+PS (Asia Pacific) Plating grade, primarily automotive applications. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EM7100 PPE+PS Automotive interiors. 200F DTUL. Excellent processability/economy. Good impact/mechanicals vs styrenics. Trim/instrument panel components. |
|||
Izod Impact, Notched | 3.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3001MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 3.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 3.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS 3501 Black 1302 Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 3.47 J/cm @Temperature 22.8 °C |
6.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PCSP0005 Polycarbonate/ASA Alloy, Flame Retardant Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P268WO PPO An extrusion grade for general purpose application requiring flame retardancy and good impact resistance.Data provided by the manufacturer |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP LNP* STAT-KON* MFD03 is a compound based on Polypropylene resin containing 15% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific) LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PREVEX W20 PPE+PS Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Izod Impact, Notched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA12 1100 Tungsten Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Tungsten FillerInformation provided by TP Composites, Inc. |