Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 TPEE (Asia Pacific) LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber. |
|||
Izod Impact, Notched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA Blowmolding and extrusion. High heat and chemical resistant. |