Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.20 J/cm @Temperature 23.0 °C |
6.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer Available in North America Recycled Content: Yes Features: CopolymerColor: Black Form: Pellets Information provided by Ravago |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | |
Saint-Gobain Rulon® E Grade Bearing/Seal PTFE
(discontinued **) Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and .. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers PC/PBT-0820 Polycarbonate+PBT, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | |
Saint-Gobain Rulon® AMR Bearing/Seal PTFE Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon .. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS FR 2810 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PP CO FR-N Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics ABS448T Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® A100 ABS Molding Resin Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501 Natural 1000 P Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501E Natural 1000 S Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501E Natural 1050 Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
Colorite Polymers 2010 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 3.20 - 4.27 J/cm | 6.00 - 8.00 ft-lb/in | |
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Izod Impact, Notched | 3.20 - 4.81 J/cm | 6.00 - 9.00 ft-lb/in | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Izod Impact, Notched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
PlastxWorld CEVIAN® A1300 PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.Information provided by PlastxWorld Inc. |