Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Nylene® 451 Nylon 6, 50% RH Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Nylene® 454 Nylon 6, 50% RH Injection molding grade. Nylene 454 is the heat stabilized version of 451 recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistanc.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Nylene® 600 Nylon 6, 50% RH, Extrusion Grade Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacketing and centrif.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Nylene® 601 Nylon 6, 50% RH, Extrusion Grade Extrusion grade. Nylene 601 is the heat stabilized version of 600 which is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other app.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Nylene® 607 Nylon 6, 50% RH, Extrusion Grade Extrusion grade. Nylene 607 is a very high viscosity extrusion resin having an ASTM relative viscosity of 800. Nylene 607 has excellent structural strength, durability, and physical properties. It .. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Nylene® 609 Nylon 6, 50% RH, Film/Extrusion Grade Film Grade. Nylene 609 is a high viscosity, extrusion resin recommended for practically all types of extrusion including profile, film, and extrusion coating. It is especially recommended for
fl.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256-56 |
Rotuba 870 Ethyl Cellulose Data provided by the manufacturer. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G.. |
|||
Izod Impact, Notched | 3.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC) Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhance.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Izod Impact, Notched | 3.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.81 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm Notch Depth; ASTM D256 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 114WO PBT Polyester A high impact polyester with low shrinkage, flame retardant.Data provided by the manufacturer |
|||
Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |