Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.94 J/cm @Temperature 23.0 °C |
5.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers SOFTAPLAS™ R 60300 GF Nat Thermoplastic Polyurethane, 30% Glass Fiber 30% short glass fiber reinforced for excellent strength and processabilityAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256 |
I. Stern 750 Medium Impact Black ABS Features:Easy color-abilityInjection MoldingApplicationsOffice equipmentElectronic partsSpools, ReelsInformation provided by I. Stern & Co. Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | |
MTI ThermoStran® PP-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256 |
Multibase Multi-Flamâ„¢ 0501 PP Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionBlow MoldingUses:TubingPipingInformation provided by Multibase |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 LGF50 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityUL File Number: E15731.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256 |
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256 |
Total HDPE BM962 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature -40.0 °C |
5.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501 Natural 1050 Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3502 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3502E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256A |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501 HF Description: High FlowInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | molded and tested in accordance with ASTM D 4101; ASTM D256A |
Dow 6D83K Polypropylene Resin DOW 6D83K is intended for use in extrusion blow molding processes where enhanced clarity is desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July .. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SBB 3710 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provide.. |