Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MGABS02 ABS General purpose ABS. Excellent flow/impact. |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® BDT5510 ABS Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only. |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific) Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
Izod Impact, Notched | 2.93 J/cm | 5.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EZ250 PPE+PS Automotive wheel covers. Offers superior processability/flow and better chemical resistance when exposed to many automotive fluids over PX0844. |