Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.78 J/cm | 5.21 ft-lb/in | Approximation; ISO 180/1U |
Albis Plastics Tedur® L V 9113-2 PPS, 60% Glass Fiber
(discontinued **) Glass Fiber Grade with Highest Mechanical Strength and Stiffness. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Housings for Shock Absorbers and Spring ElementsProce.. |
|||
Izod Impact, Notched | 2.78 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.21 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS 4501 Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 2.78 J/cm | 5.21 ft-lb/in | ASTM D256 |
Bapolene® 2035 Polyethylene, Blow Molding Grade Bapolene HD2035 is a high density polyethylene copolymer for blow molding applications. It is recommended for applications that require high top load strength and good ESCR properties. This produc.. |
|||
Izod Impact, Notched | 2.78 J/cm @Temperature 23.0 °C |
5.21 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East) LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |