Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Nylene® Norpex® AX245 PPE (Polyphenylene Ether) Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Network Polymers NPP 25-0105 TF20 Description: Copolymer Polypropylene, 20% Talc FilledInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | |
Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26FX100 is a general-purpose extrusion grade with mechanical properties that classify it as an eng.. |
|||
Izod Impact, Notched | 2.40 J/cm @Temperature -30.0 °C |
4.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 2.40 J/cm @Temperature 22.8 °C |
4.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP7130 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Izod Impact, Notched | 2.40 - 2.94 J/cm @Thickness 3.17 mm |
4.50 - 5.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM Data |
Styron Magnum™ 780HP ABS, High Heat, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Izod Impact, Notched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® ABS CR X Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.40 J/cm @Temperature 23.0 °C |
4.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl EN130P PPE+PS (Asia Pacific) High heat, extrusion grade PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N130GL (COND, 50% RH) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic.. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Izod Impact, Notched | 2.40 J/cm @Temperature -40.0 °C |
4.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
Izod Impact, Notched | 2.40 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS 2501 Injection Molding Grade, Medium Impact, High Flow Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® PPO 263 A general purpose grade with good heat resistance and impact strength. Other properties include dimensional stability and moisture resistance.Data provided by the manufacturer |
|||
Izod Impact, Notched | 2.40 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
4.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(discontinue Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N233GL (COND, 50% RH) Nylon 6, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R12 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC (Asia Pacific) LNP LUBRICOMP* DL002 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 2.40 - 6.70 J/cm | 4.50 - 12.6 ft-lb/in | Average value: 4.20 J/cm Grade Count:7 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |