Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.1356 - 4.59154 J/cm @Temperature -40.0 - 93.3 °C |
4.0009 - 8.60184 ft-lb/in @Temperature -40.0 - 200 °F |
Average value: 3.36 J/cm Grade Count:2 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 2.1356 - 9.12969 J/cm @Temperature 0.000 - 0.000 °C |
4.0009 - 17.1037 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 5.63 J/cm Grade Count:2 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 2.1356 - 9.12969 J/cm @Diameter 6.35 - 6.35 mm |
4.0009 - 17.1037 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 5.63 J/cm Grade Count:2 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Temperature -40.0 - -30.0 °C |
4.0009 - 4.0009 ft-lb/in @Temperature -40.0 - -22.0 °F |
Average value: 3.16 J/cm Grade Count:3 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Thickness 3.17 - 3.20 mm |
4.0009 - 4.0009 ft-lb/in @Thickness 0.125 - 0.126 in |
Average value: 3.16 J/cm Grade Count:3 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Temperature -28.9 - -28.9 °C |
4.0009 - 4.0009 ft-lb/in @Temperature -20.0 - -20.0 °F |
Average value: 1.09 J/cm Grade Count:1 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Thickness 3.17 - 3.17 mm |
4.0009 - 4.0009 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.09 J/cm Grade Count:1 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |