Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N2033STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256A |
Dow INSPIRE™ TF2300 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | |
Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive Mix ratio 2 to 1 by volume.TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications whe.. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | at 73°F; ASTM D256 |
M. Holland Company CP502 Polypropylene Copolymer Features: Copolymer, High Flow, High Impact ResistanceUses: Closures, Medical Applications, Thin-walled PartsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | ASTM D256 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF25 IM L 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN133GTL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene Impact Copolymer for Extrusion Applications Formolene® 2302E is a low flow, medium impact polypropylene copolymer designed for extrusion applications. It is a barefoot resin with a basic stabilizat.. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D-256-92 |
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, perm.. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3500ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3502ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | >= 2.14 J/cm | >= 4.00 ft-lb/in | ASTM D256 |
Dow UNIPOL™ DGDA-5110 Polyolefin DGDA-5110 UNIPOL™ is designed for the manufacture of thermoformed truck liners and other sheet extrusion applications requiring toughness and good process-ability. Information provided by Dow |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436G40CL Glass Reinforced |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | Crosswise; ASTM D256 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Amco Amalloy® B1017A Clear Multipolymer Alloy Amco Amalloy B1017A is a high impact multipolymer with exceptional clarity, good tensile and flexural strength, and medium-high melt flow.Super high impact, medium melt flow, good tensile and flexur.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Izod Impact, Notched | >= 2.14 J/cm | >= 4.00 ft-lb/in | ASTM D265 |
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa.. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |