Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 18.7 J/cm | 35.0 ft-lb/in | ASTM D256 |
Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC Lytex 9063 is a high performance, glass fiber reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention.. |
|||
Izod Impact, Notched | 18.7 J/cm | 35.0 ft-lb/in | ASTM D256 |
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC
(discontinued **) QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st.. |