Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.02 J/cm @Temperature -30.0 °C |
3.78 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact |
|||
Izod Impact, Notched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Izod Impact, Notched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific) High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Izod Impact, Notched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Izod Impact, Notched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PS+PA High flow PPE+PS+PA for under-the-hood and electrical applications. With mold release |
|||
Izod Impact, Notched | 2.02 J/cm @Temperature 23.0 °C |
3.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |