Polymer Property : Izod Impact, Notched = 3.29 ft-lb/in
Polymer Property :
Izod Impact, Notched =
3.29 ft-lb/in
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Notched
1.76
J/cm
3.29
ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 2520 XU Black Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase