Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.6017 - 1.6017 J/cm @Temperature -28.9 - -28.9 °C |
3.0006 - 3.0006 ft-lb/in @Temperature -20.0 - -20.0 °F |
Average value: 1.60 J/cm Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |