Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
Omni Plastics OmniLon™ 6 PA6 IM20 Unfilled/ Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
Omni Plastics OmniLon™ 6/6 PA6/6 IM20 Unfilled/ Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | edgewise; ASTM D256 |
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced The 44500 series sheet molding compound offers high strength and excellent resistance to corrosive agents. This compression molding grade is formulated with a vinyl ester resin system. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | edgewise; ASTM D256 |
Haysite 48600 Polyester SMC, 30% Glass Reinforced The 48600 series sheet molding compound is formulated with a high temperature resin system (180º C). Designed for compression molding, this grade offers excellent retention of physical and electr.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256-92 |
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy Stat-Rite® M-690 is a static dissipative PETG alloy. Stat-Rite® M-690 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Izod Impact, Notched | 10.7 J/cm @Thickness 3.17 mm |
20.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Formosa Plastics Formolon® APW Compound APW Powder Window Profile Compound Series The APW compounds have been designed for profile extrusion in window lineals, fencing and other outdoor weatherable markets. It exhibits excellent whiteness.. |
|||
Izod Impact, Notched | >= 10.7 J/cm | >= 20.0 ft-lb/in | |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
Izod Impact, Notched | >= 10.7 J/cm | >= 20.0 ft-lb/in | |
TriStar Ultracomp UC-300 Composite Bearing Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family.. |
|||
Izod Impact, Notched | >= 10.7 J/cm | >= 20.0 ft-lb/in | |
TriStar Ultracomp UC-400 Composite Bearing Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry .. |
|||
Izod Impact, Notched | <= 10.7 J/cm | <= 20.0 ft-lb/in | |
TriStar Ultracomp UC-500 Composite Bearing Ultracomp UC-500 - Multiple sources of lubrication make this Ultracomp an excellent choice for full rotary or higher speed linear applications. High strength, high impact resistance and long wear li.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
Applied Composites 8061 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped Fibers, High Stiffness, High Fiber LoadingsInformation provided by Applied Composites Corp.. |
|||
Izod Impact, Notched | 10.7 J/cm @Thickness 3.17 mm |
20.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 7045 Rigid PVC, Extrusion Georgia Gulf 7045 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 847 Nylon 6, Film Grade A very high impact, low flexural modulus Nylon 6 resin for molding or extrusion. Outstanding low temperature properties.Data provided by the manufacturer |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Izod Impact, Notched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
Applied Composites 8057 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Carbon/Glass Fibers, Advanced Composite Structures, Ribs and Flat Surfaces, High ModulusInformation provided by App.. |