Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.53 - 3.2034 J/cm @Temperature -40.0 - -30.0 °C |
2.87 - 6.0013 ft-lb/in @Temperature -40.0 - -22.0 °F |
Average value: 2.37 J/cm Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 1.53 J/cm @Temperature 23.0 °C |
2.87 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Flint Hills AP6835-HS Polypropylene Impact Copolymer Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resource.. |
|||
Izod Impact, Notched | 1.53 J/cm @Temperature -30.0 °C |
2.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Izod Impact, Notched | 1.53 J/cm @Temperature -30.0 °C |
2.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Izod Impact, Notched | 1.53 J/cm | 2.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |