Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7189 PC Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1200 A 43 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | Conditioned; ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ISO 180 |
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
&n Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 0.000 °C |
2.81 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10312 PA (Asia Pacific) 9X10312 is 50% glass fiber reinforced, impact modified nylon material. High modulus, high flow and good ductility, Low Moisture Absorption. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA250G45 , 45% Glass Fiber Reinforced PA66, DAM 45% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM 15% GF reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -40.0 °C |
2.81 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 527 Nylon 66 A very high impact, slightly lubricated, nylon resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced 6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
Styrolution Luran® S KR 2867 C WU Colored ASA+PC Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256A |
LyondellBasell Astryn 6652 Polypropylene Homopolymer Key Features: low melt flow, medium modulus polypropylene homopolymer, high strength, high impact, good hydrolytic abilityApplications: water pipe fittings and connectorsDescription: Astryn 6652 low.. |