Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.42 J/cm @Temperature 23.0 °C |
2.66 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Izod Impact, Notched | 1.42 J/cm | 2.66 ft-lb/in | ASTM D256 |
Cheng Yu Plastic A702G1 ABS 10% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 1.42 J/cm @Temperature -30.0 °C |
2.66 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended. |