Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | ASTM D256 |
Nylene® 9110 G33 , 33% Glass Reinforced Nylon 6/10 Description: Nylene® 9110 G33 is a 33% glass fiber reinforced nylon 6/10. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour.. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | ASTM D256 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 22.8 °C |
2.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 22.8 °C |
2.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® FPI-33 BK Nylon 6, 33% Glass Reinforced, post industrial Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 409 L MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | ASTM D256 |
Techmer ES Electrafil® ABS-1200/SD/FR BL ABS |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® ABS-1251/SD ABS, Static Dissipative Polymer Alloy |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -28.9 °C |
2.50 ft-lb/in @Temperature -20.0 °F |
ASTM D256 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PA6/6 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | ASTM D256 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | ISO 180/A |
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS TM 25 Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 22.8 °C |
2.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA211G40 Nylon 6, 40% Glass Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ MP-20GF/05T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® AM 33 GF/000 L HS Black Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Heat StabilizedBlackEnhanced LubricationGlass Fiber ReinforcedInformation provided by PolyOne Corporation. |