Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.49 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC (Asia Pacific) LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C2805 PC+ABS LNP* Lubricomp* Cycoloy* C2805 compound is a PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX07404H PC LNP* LUBRICOMP* DX07404H is a compound based on Polycarbonate containing Proprietary Fillers. Added features of this grade are: Healthcare, Wear Resistant. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RF208 PA 66 LNP LUBRILOY* RF208 is a compound based on Nylon 66 resin containing 40% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM Data |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PN235 PPE+PS Plating grade, primarily automotive applications. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PX1265 PPE+PS (Asia Pacific) Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PX1391 PPE+PS (Asia Pacific) Automotive applications, primarily. Excellent electrical properties. high heat. 305F (152C) DTUL. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM Data |
Styron Magnum™ 347EZ ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PX0888 PPE+PS (Asia Pacific) Unfilled, non-FR. Higher heat resistance than N110 (BOZ) and px0844 (USA). For automotive interiors. 250F (121C) DTUL. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.49 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS 3500 ELG Natural 1003 Injection Molding Grade, High Flow, Medium Impact, Low Gloss Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PP-CP10/2 Impact Copolymer, 10 Melt Flow, Nucleated, Anti-stat This product is intended for injection molding applications such as consumer products, toys, housewares, office furniture, and juvenile products.Information provided by Entec |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® D926 Nylon 12 A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl.. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 213 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.33 J/cm @Diameter 3.17 mm |
2.49 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5540 High Impact Polystyrene
(discontinued **) Excellent balance of toughness, flow, and set-up, High gloss, USP Class VIApplications: Structural foam, Housewares, Toys, Appliance parts, Dairy containersProperties were determined on injection mo.. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM Data |
Styron Magnum™ AG700 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content. |
|||
Izod Impact, Notched | 1.33 J/cm | 2.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 23.0 °C |
2.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10 (Asia Pacific) LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |