Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
NYCOA 27/300SR Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 H-B nylon 6Information provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
NYCOA 5033 HS 33% Glass-Fiber Reinforced, Heat Stabilized, Nylon 66 Resin NYCOA 5033 HS is a 33% glass fiber reinforced, heat stabilized Nylon 66 resin used for injection molding. It offers an outstanding balance of mechanical properties over standard grades of convention.. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Nylene® 402 Nylon 6 Injection molding grade. Dry as molded. Nylene 402 is a high monomer resin which offers outstanding toughness and flexibility. Nylene 402 exhibits excellent flow properties at temperature and press.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ ND633 GF Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.18 mm |
2.44 ft-lb/in @Thickness 0.125 in |
Injection Molded, 3.6 mm Notch Depth; ASTM D256A |
PolyOne Nymax™ NM 6600-44GF0001 White Polyamide 66 (Nylon 66) The Nymax® GMF 1200 Series of compounds are based upon nylon 6/6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part per.. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -29.0 °C |
2.44 ft-lb/in @Temperature -20.2 °F |
|
Spartech Spectrum® S370 TPO Polyolefin Sheet
(discontinued **) Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.17 mm |
2.44 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® FV-30 Nylon 6, 30% Glass Reinforced, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.17 mm |
2.44 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® FV-31 Nylon 6, 31% Glass Reinforced, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | 23° C; ASTM D256 |
Flint Hills AP6412-HS Impact Copolymer Polypropylene High impact copolymer, and FDA compliant. Features: Blush resistant and heat stabilized.Applications: Injection molding: consumer durables, automotive interior trim, furniture trim and housing, and .. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Kuraray Genestarâ„¢ GW1458HF Nylon, 45% Glass Filled Low Warpage, High Flow HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -20.0 °C |
2.44 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Spartech Royalite R59M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. A unique ABS/PVC resin that meets the flammability standards of many industries and is a cost-effective alternative to standard fire-rated ABS. High rigidity in t.. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature 23.0 °C |
2.44 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough RZ300G6 Polycarbonate, 30% Glass Fiber 30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature 23.0 °C |
2.44 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough RZ310G6 Polycarbonate, 30% Glass Fiber 30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
E-Polymers TEKANATE™ G720 , 20% Glass Fiber Reinforced Poly Carbonate 20% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SG-2 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 4233 B ABS Utility GradeABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of proces.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Adell BT-14 Nylon 6, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256A |
LyondellBasell Astryn 7523C Polypropylene Copolymer Key Features: conventional melt flow, medium modulus polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, versatile, good processabilityApplications: autom.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature 23.0 °C |
2.44 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |