Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific) Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66 High thermal resistant, Weather resistant, dimensionally stableApplications Cylinder head coversInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature 23.0 °C |
2.38 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature 23.0 °C |
2.38 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® EPC40R Polypropylene impact copolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature 23.0 °C |
2.38 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature -30.0 °C |
2.38 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN3L PPE+HIPS (Asia Pacific) PPE+PS, GF30%, hydrolytic stability improved |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
Unitika M1030DH PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 13G43 43% Glass Filled Nylon 66 43% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Mechanical and electrical parts such as micromotors, automotive parts such as radiator tanks and shift leversInformation provi.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66 Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |