Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.17 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature 22.8 °C |
2.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature 22.8 °C |
2.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylex® P1010G7FRMA Polycarbonate, 7% Glass Filled Polycarbonate, 7% Glass Filled, Flame RetardantInformation provided by Ravago. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers GPP-230 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers GPP-240 Homopolymer Polypropylene, 40% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF33 L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackTPCI# 8221102Information provid.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF8 IM3 BK 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubric.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF30 IM 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PlastxWorld CEVIAN® A5624 20% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PC310GR Polycarbonate (Utility Grade), 10% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Total PSI 845E Polystyrene Polystyrene 845E is a high impact polystyrene specially designed for the custom sheet market. The polymer produces tough, ductile sheet with a rich matte finish. This material is especially suitable.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437T20L Talc Reinforced |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |