Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.10 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Nylene® PA6 Glass Filled 5233 HS Nylon 6 33% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Nylene® PA6 Glass Filled 5243 HS Nylon 6 43% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® PK-30GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
PolyOne Geon™ CPVC EC050 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC050 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon EC050 demonstrates ease of processing and excellent t.. |
|||
Izod Impact, Notched | 1.10 - 1.10 J/cm @Temperature -40.0 - -40.0 °C |
2.06 - 2.06 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.10 J/cm Grade Count:1 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **) Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | reverse notched; ASTM D256 |
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® AT-000/000 HI5 Natural NA Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Kolon KOCETAL® EL304 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Loxim 430 01HB Nylon 6,6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -29.0 °C |
2.06 ft-lb/in @Temperature -20.2 °F |
|
Spartech Royalite R84 Proprietary Polymer Weather Resistant Sheet Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ISO 180/A |
Styron CALIBREâ„¢ 7102-8 Polycarbonate CALIBREâ„¢ 7102-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Acudel® 22000 Polyphenylsulfone, Modified (PPSU, Modified) Acudel® 22000 is a modified polyphenylsulfone. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases and good re.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm |
2.06 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SH 731 High Impact Polystyrene Characteristics Medium flow High Impact Excellent formability Low temperature toughnessProcessing Extrusion Molding FormingApplications Thermoformed containers, extruded profiles, packaging pro.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ300G3 Polycarbonate, 15% Glass Fiber 15% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epinyl PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre, excellent mechanical properties |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® N6030FR 30% Glass Fiber Reinforced Flame Retardant Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
Adell BW-17 Nylon 6, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |