Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.068 J/cm @Temperature 23.0 °C |
2.001 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Opnyl OP66GF43 Nylon 66, As Conditioned Nylon 66-Glass reinforced(43%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers |
|||
Izod Impact, Notched | 1.068 J/cm @Thickness 3.17 mm |
2.001 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers GPP-220 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.068 J/cm @Temperature 23.0 °C |
2.001 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
MRC Polymers NAXELL™ PC110-20G General Purpose Polycarbonate, Medium Viscosity, 20% Glass Fiber • Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 1.068 J/cm @Thickness 3.17 mm |
2.001 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers ABS TR-5000 Transparent Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |