Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.608 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
18.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1201-05 Polycarbonate Resin Description: LUPOY PC 1201-05 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Izod Impact, Notched | 9.608 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
18.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1261-03 Polycarbonate Resin Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista.. |
|||
Izod Impact, Notched | 9.608 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
18.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
Izod Impact, Notched | 9.608 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
18.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1600-03 Polycarbonate Resin Description: LUPOY PC 1600-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Izod Impact, Notched | 9.608 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
18.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1603-03 Polycarbonate Resin Description: LUPOY PC 1603-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Izod Impact, Notched | 9.608 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
18.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |