Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.13 J/cm | 17.1 ft-lb/in | ASTM D256 |
Kolon Kopa® KN151 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 9.11 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
17.1 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polyethylene Terephthalate (PET) resin matrix. This composite material fea.. |