Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.99 J/cm @Temperature -30.0 °C |
16.8 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer |
|||
Izod Impact, Notched | 8.99 J/cm @Temperature -30.0 °C |
16.8 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer |
|||
Izod Impact, Notched | 8.99 J/cm @Temperature -30.0 °C |
16.8 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 8.99 J/cm @Temperature -30.0 °C |
16.8 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 8.99 J/cm @Temperature -30.0 °C |
16.8 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 8.99 J/cm @Temperature -30.0 °C |
16.8 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer 7 MFR LEXAN HFD Copolymer |
|||
Izod Impact, Notched | 8.97 J/cm | 16.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Izod Impact, Notched | 8.97 J/cm | 16.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |