Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 2502 C Natural Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers PC 714-FR Series PC, Flame retardant Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Global PC-1415-GY-802-R General Purpose Gray Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Global PC-1415-R General Purpose Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Global PC-1418 General Purpose Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® PCT2010 PC/PCT Alloy, Chemical Resistant PC/PCT alloy with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
0.125"; ASTM D256 |
LTL Color Compounds ColorRxâ„¢ PC-1002ARX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PBT IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | >= 8.54 J/cm @Thickness 3.17 mm |
>= 16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 L UV (Conditioned) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 603 3 Polycarbonate, Branched CALIBRE® 603 is a branched polycarbonate resin and is equipped with a mold release and a UV stabilization package. CALIBRE 603 resins exhibit an excellent property balance of high clarity, high m.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 701 15 Polycarbonate, General Purpose CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resi.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 603 5 Polycarbonate, Branched CALIBRE® 603 is a branched polycarbonate resin and is equipped with a mold release and a UV stabilization package. CALIBRE 603 resins exhibit an excellent property balance of high clarity, high m.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N100STL (DAM) Nylon 6, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PC100HFR Polycarbonate Molding Resin, High Flow, Mold Release Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 8.54 - 9.08 J/cm | 16.0 - 17.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PC100R Polycarbonate Molding Resin, Mold Release Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 8.55 J/cm | 16.0 ft-lb/in | ASTM D256 |
DuPont™ Surlyn® 8660 Ionomer Resin, Sodium Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Entec Hylex® P1007L1 HB Polycarbonate Available in North America Agency Ratings: FDA 21 CFR 177.1580 RoHS Compliant Form: Pellets Information provided by Entec |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® TD930H Nylon 12 A plasticized Nylon 12 offering outstanding flexibility with superior moisture and chemical resistance, UV and heat stabilized for weatherability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® AEN 6600-3 Nylon 6/6 Engineered Resin |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® PP CO 99074 Availability: North AmericaForms: PelletsFeature: Copolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
PlastxWorld CEVIAN® A1500 PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc. |