Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.66 J/cm | 10.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 5.66 J/cm | 10.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 5.65 J/cm | 10.6 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.65 J/cm | 10.6 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.65 J/cm | 10.6 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.65 J/cm | 10.6 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.65 J/cm | 10.6 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.66 J/cm | 10.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 5.66 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
10.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS/PC 9801 Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 5.65 J/cm | 10.6 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.66 J/cm | 10.6 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® PC/ABS Alloy 305 General purpose high gloss with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |