Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -40.0 °C |
10.5 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific) High impact, extrusion grade polycarbonate/ABS alloy. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
Ineos B35-150-134 MDPE
(discontinued **) Fortiflex® B35-150-134 is an intermediate density polyethylene copolymer developed for injection blow molding. It exhibits excellent gloss and environmental stress crack resistance (ESCR) in molde.. |
|||
Izod Impact, Notched | >= 5.59 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 10.5 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HI5002A PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched | 5.59 J/cm @Thickness 3.17 mm |
10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.59 J/cm @Thickness 3.17 mm |
10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.61 J/cm @Thickness 3.17 mm |
10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature 23.0 °C |
10.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.61 J/cm | 10.5 ft-lb/in | ASTM D256A |
Dow INSPIRE™ 117.00 Performance Polymer 117.00 Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity a.. |
|||
Izod Impact, Notched | 5.60 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
10.5 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Izod Impact, Notched | 5.61 J/cm | 10.5 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437C20L Calcium Reinforced |
|||
Izod Impact, Notched | 5.61 J/cm | 10.5 ft-lb/in | ASTM D256 |
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded .. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256A |
Braskem INSPIRE™ 117 Performance Polypropylene Polymer D 117.00 Developmental Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistanc.. |