Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific) High flow PC+ABS. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXM121R PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC (Asia Pacific) LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412HF PC 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific) LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC (Asia Pacific) LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific) LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA 30% Glass Reinforced PPE+PA Alloy. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp DF0066P PC LNP THERMOCOMP* DF0066P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing.This data was supplied by.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -40.0 °C |
1.99 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL BN31 PPE+PS Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 133 G Nylon 66, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 66 offering excellent high temperature performance, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile .. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412HF PC (Asia Pacific) 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6 LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |