Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.01441 - 5.30 J/cm @Temperature -40.0 - -10.0 °C |
1.90041 - 9.93 ft-lb/in @Temperature -40.0 - 14.0 °F |
Average value: 2.90 J/cm Grade Count:39 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 1.01441 - 5.30 J/cm @Thickness 3.17 - 6.35 mm |
1.90041 - 9.93 ft-lb/in @Thickness 0.125 - 0.250 in |
Average value: 2.90 J/cm Grade Count:39 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 1.01441 - 1.01441 J/cm @Temperature -40.0 - -40.0 °C |
1.90041 - 1.90041 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 2.55 J/cm Grade Count:1 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Notched | 1.01441 - 1.01441 J/cm @Thickness 3.17 - 3.17 mm |
1.90041 - 1.90041 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 2.55 J/cm Grade Count:1 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Notched | 1.01441 - 1.01441 J/cm @Temperature -40.0 - -40.0 °C |
1.90041 - 1.90041 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.01 J/cm Grade Count:1 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 1.01441 - 1.01441 J/cm @Thickness 3.17 - 3.17 mm |
1.90041 - 1.90041 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.01 J/cm Grade Count:1 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 1.01441 - 1.33475 J/cm @Temperature -40.0 - -40.0 °C |
1.90041 - 2.50053 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.20 J/cm Grade Count:7 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |