Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.87 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2710 TRN 9470 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific) Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MP 90 High Density Polyethylene - Injection Molding Eraclene MP 90 is a high density polyethylene homopolymer resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MP 90 has a narrow molecular weight distribution and a h.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Izod Impact, Notched | >= 1.00 J/cm @Temperature 23.0 °C |
>= 1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 1401D (Q30P) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Gichem GILAC G160 Acrylonitrile Butadiene Styrene
(discontinued **) ABS very high fluidity, good resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Gichem GILAC D160/MT Acrylonitrile Butadiene Styrene
(discontinued **) ABS with good resilience, good thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
Loxim 230 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific) PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump .. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber 15% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.17 mm |
1.87 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB320G3 Nylon 6, 15% Glass Fiber, Flame Retardant 15% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PD300G4 Nylon 12, 20% Glass Fiber 20% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPC500 Polypropylene, Flame Retardant Flame retardant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® G70GR , 30% Glass Reinforced PC/ABS Alloy 30% Glass Fiber reinforced, High stiffness, Dimensional stabilityInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.00 J/cm @Diameter 3.17 mm |
1.87 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Acclear® 8449 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlTypical applications: Housewares, Rigid packagingComplies wit.. |