Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.960 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU) Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne |
|||
Izod Impact, Notched | 0.960 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® NN-30GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | |
CE Phenolic Laminate Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® NL-30GF/000 FR Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Kostat ICP-STAT ICS-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -40.0 °C |
1.80 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific) LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific) LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC (Asia Pacific) LNP* THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP OF008H PPS - Linear LNP* THERMOCOMP* OF008H is a compound based on PPS - Linear containing 40% Glass Fiber. Characteristics of this grade are: Healthcare. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRP 5902 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Gloss; High Impact Resistance Uses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® VGR30 30% GF ABS Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle.. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature 22.8 °C |
1.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA2SP0004 Nylon 6 Alloy Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced A 25% mineral reinforced, 15% glass fiber reinforced nylon 6 offering excellent rigidity, dimensional stability and warpage control in large area parts.Data provided by the manufacturer, Chem Polyme.. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Cheng Yu Plastic E2345 Flame Retardant PET, 45% Glass Fiber |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P1-20FG-2703 20% Glass Fiber Reinforced, Impact Modified Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |