Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP521-187 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9779 Medium Grey Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® PI-30GF/000 Polyether Imide (PEI) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.910 - 7.50 J/cm @Temperature -40.0 - -40.0 °C |
1.70 - 14.1 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 2.61 J/cm Grade Count:3 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® PK-15CF-15GB/000 Polyetheretherketone (PEEK), Glass Bead, Carbon Fiber Reinforced
(discontin Description/Features:Carbon Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | Injection Molding; ASTM D256 |
Network Polymers 351 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | 73°F; ASTM D256 |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436W40L1 Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 624 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.43% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® L935 Nylon 11 An economy grade, unplasticized Nylon 11 for extrusion applications. Also available is L935H, same with UV and heat stabilizer.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |