Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.840 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.57 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1383 PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Notched | 0.840 J/cm @Temperature -30.0 °C |
1.57 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Izod Impact, Notched | 0.840 J/cm @Temperature -30.0 °C |
1.57 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 0.840 J/cm @Temperature -30.0 °C |
1.57 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 0.840 J/cm @Temperature -30.0 °C |
1.57 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 0.838 J/cm @Thickness 3.20 mm |
1.57 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HI 450S High Gloss HIPS Key features: High-gloss Common Uses: Portable CD-case, air conditioner cases.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impac.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6 LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Notched | 0.840 J/cm @Temperature 23.0 °C |
1.57 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp RFN18SXZ PA 66 LNP LUBRICOMP* RFN18SXZ is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Ameri.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AR002XXH ABS LNP* THERMOCOMP AR002XXH is a compound based on ABS resin containing 10% Barium Sulfate. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6 LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific) PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Izod Impact, Notched | >= 0.840 J/cm | >= 1.57 ft-lb/in | Method A; ASTM D 256 |
Karina E 837-10/68-Y-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
Custom Resins Vexel™ 4200 RD PBT; 30% Glass Filler
(discontinued **) Property data for dry as molded samples.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
Plenco 51030 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued.. |
|||
Izod Impact, Notched | 0.840 J/cm | 1.57 ft-lb/in | ASTM D256 |
Plenco 50030 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |