Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.779 J/cm | 1.46 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ ABS GRC10 NA Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LGN1500 PC (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SP7604 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KG-15MRA Polycarbonate, 15% Glass Fiber Reinforced Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KGN-15MRA Polycarbonate, Flame Retardant, 15% Glass Fiber Reinforced Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® AB9530 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature -30.0 °C |
1.46 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® PDR4910 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature -30.0 °C |
1.46 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® SHF434HR PBT PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXQ PEI LNP* THERMOCOMP* EC004XXQ is a compound based on Polyetherimide containing 20% Carbon Fiber. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7604 PC (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WF007 PET/PBT LNP Thermocomp WF-1007 BK8-114 is a compound based on PET/PBT resin containing glass fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL INT1001 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, high flow for auto interior |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL LEN2211 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, FR for LED application |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N802 PPE+HIPS (Asia Pacific) PPE/PS 80oC V2 FR high flow |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PCN2615 PPE+PS (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2956 PPE+PS (Asia Pacific) PPE+PS GF+Mineral Filler total 35% FR V-0 |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V8280SF PBT+PET High Modulus, PBT+PET, 40% Glass Reinforced, Mold Release, Super High Flow |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL APS430 PPE+PPS (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East) Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Izod Impact, Notched | 0.780 J/cm @Thickness 3.17 mm |
1.46 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 925-20PF Nylon 12, PTFE Lubricated 20% filled PTFE lubricated, Nylon 12.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |