Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Izod Impact, Notched | >= 0.750 J/cm @Temperature 23.0 °C |
>= 1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 7445L (EPC57MA) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC CC862 High Density Polyethylene for Injection Molding Product Description: SABIC HDPE CC862 is a high density polyethylene specially developed for still water bottle caps that meet organoleptic properties requirements. The material offers and ideal c.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Edistir RKL Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA66-RG001 Flame Retardant PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation Provided by Kingf.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PET-G15 15% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 0.000 °C |
1.41 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 0.000 °C |
1.41 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -20.0 °C |
1.41 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® K3501 PBT (Europe-Africa-Middle East) Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.750 J/cm @Temperature 23.0 °C |
>= 1.41 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA300G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH353M8 Polypropylene, 40% Mineral Filled 40% mineral filled polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamSter RF300G4 PBT, 20% Glass Fiber 20% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar AN004 Natural PCTA Copolyester EASTAR AN004 Copolyester contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exp.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ASA TW18B3 ASA Weatherable Polymers Injection Molding Grade, Very High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® T80GFR , Flame Retardant, 30% Glass Fiber Reinforced PBT/ABS Alloy 30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm |
1.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® 304-G30 PBT Resin 30% glass fiber reinforced, flame retardant, low bleeding, UV-resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 463 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | 0.5 in.; ASTM D256 |
Resirene Resirene® 2210 High Impact Polystyrene Features:Very High FlowEasy ProcessingGood GlossFlexibilityFDA Rating: 21 CFR 177.1640High ProductivityApplications:InjectionThin Wall ApplicationsHard to Fill MoldsTelephonical DevicesYot CupsToysC.. |