Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ISO METHOD 180 |
NYCOA 2237 Copolymer Nylon 6/66 Alloy transparent molding and extrusion gradeInformation provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Kadel® E-1300 Polyketone
(discontinued **) High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Izod Impact, Notched | 0.700 - 3.7373 J/cm @Temperature -40.0 - -20.0 °C |
1.31 - 7.0015 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 2.22 J/cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Izod Impact, Notched | 0.700 - 5.07 J/cm | 1.31 - 9.50 ft-lb/in | Average value: 1.57 J/cm Grade Count:133 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer Key Features: high flow, compatible with hindered amine light stabilizers, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpageAppli.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256/ISO 180 |
Ineos Styrenics Polystyrene 147F (NAFTA) An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -20.0 °C |
1.31 ft-lb/in @Temperature -4.00 °F |
|
Kuraray SEPTON® PM1 Polypropylene Modified Plastic Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Unitika M1030E PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA301G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1003 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epinyl PA 66 GF 30 H Polyamide 66, 30% Glass, Heat Stabilized Characteristics: 30% glass fibre filled |
|||
Izod Impact, Notched | 0.700 - 1.30 J/cm @Thickness 6.35 mm |
1.31 - 2.44 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATISHIELD 90/13-07A-V1 Modified Polyphenylene Oxide (PPOm) Base E.M.I. Shielding Plastic (UL94 V-1)
(di Description: Latishield E.M.I. shielding materials were developed to solve the problem of shielding electromagnetic interferences with plastic components. The answer is a mixture of two different ty.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Asia Pacific) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.17 mm |
1.31 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Washington Penn PPC7UF0-Black Polypropylene, High Flow Copolymer Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.Data provided by Washington Penn Plastic Co., Inc. |
|||
Izod Impact, Notched | 0.700 J/cm @Diameter 3.17 mm |
1.31 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Acclear® 8939 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Excellent static control, ToughenedTypical applications: Housewares, Rigid packaging, Media packag.. |