Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 70 High Density Polyethylene - Injection Molding Eraclene MQ 70 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MQ 70 is suggested in applications for which high creep, impact and .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and st.. |
|||
Izod Impact, Notched | 0.650 - 0.800 J/cm | 1.22 - 1.50 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced
(discontinued AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.20 mm |
1.22 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 515 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any colorProcessing Injection molding Extrusion Applications Electrical switch boards MCB distribution bo.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.17 mm |
1.22 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika C300VN Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA112NT Nylon 6.6, PTFE Filled Polyamide 66 filled with PTFE to improve wear resistance in molded partsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA325G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM3013G4 Acetal, 20% Glass Fiber 20% Glass fiber reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -20.0 °C |
1.22 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Total PPC 4624WZ Polypropylene, Impact Copolymer ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC618P PBT/PET Alloy, Anti-microbial Applications: Gas equipment partsFeatures: Good anti-microbialWarpagelessFlame resistantInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM-D256 |
Braskem GD5150K HDPE High Density Extrusion Polyethylene GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric.. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.22 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm @Diameter 3.17 mm, Temperature -20.0 °C |
1.22 ft-lb/in @Diameter 0.125 in, Temperature -4.00 °F |
bar; ASTM D256 |
BP Amoco Acctuf® 3541 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purpose, High melt flowComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded sam.. |
|||
Izod Impact, Notched | 0.650 - 2.94 J/cm | 1.22 - 5.50 ft-lb/in | Average value: 1.21 J/cm Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |