Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ HS404 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Izod Impact, Notched | 0.600 - 1.30 J/cm @Thickness 3.17 - 3.17 mm |
1.12 - 2.44 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.875 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.600 - 0.600 J/cm @Temperature 0.000 - 0.000 °C |
1.12 - 1.12 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.600 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | 23° C; ASTM D256 |
Flint Hills PP 13R9A Random Copolymer Polypropylene Random copolymer, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: Radiation resistant and good contact clarity.Applications: Injection molding: radiation sterilizab.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
Kolon KOCETAL® WR701 Wear Modified Acetal Resin Improved weather resistant and easy flow grade. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.600 - 0.650 J/cm | 1.12 - 1.22 ft-lb/in | ASTM D256 |
Loxim 235 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ISO 180 |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal RM7009 Acetal, UV Stabilized UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1419 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.12 - 1.50 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA210 LW TA210LW, Low Wear, Low Friction PA66, DAM Low wear, Low frictionInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® NC42Z Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 0.598 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Izod Impact, Notched | 0.598 J/cm | 1.12 ft-lb/in | |
Abatron AboCast 7703-21/AboCure 7703-24 (D) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |