Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 3012 RC 30% Glass Filled Polypropylene Moisture content is 0.06%. Multi-Pro 3012 RC is a glass reinforced polypropylene, chemically coupled which enhances the mechanical properties. This product has been formulated to achieve an esthe.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
NYCOA 534 H High Viscosity, Heat Stabilized Nylon 6 Resin NYCOA 534 H is a high viscosity; heat stabilized, nucleated Nylon 6 resin. The high viscosity and fast set-up time make an excellent material for extrusion of tubing, rods, sheet and film. Because o.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
NYCOA 534H PA 6 high viscosity, heat stabilized, nucleated nylon for tubing, sheet, film and moldingInformation provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded, Across Flow; ASTM D256A |
PolyOne Nymax™ 1200 A Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 600 Zip 0 Black 13 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
PolyOne Edgetek® PS-20GF/000 NATURAL Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.590 - 4.97 J/cm | 1.11 - 9.30 ft-lb/in | Average value: 1.33 J/cm Grade Count:27 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | Conditioned; ASTM D256 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac® LA531 Acetal Homopolymer, High Lubricity
(discontinued **) High-lubricity block copolymer with excellent friction and wear characteristics, especially on POM.Applications: Gears, keyboard parts.This product is not a part of the standard product line dated 2.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac®-C 7510 Acetal Copolymer, High Flow
(discontinued **) High-flow grade, suited for thin-wall, long-flow-distance moldings.Applications: Lighters, aerosol bottles, fasteners.This product is not a part of the standard product line dated 2003. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature 23.0 °C |
1.11 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Flint Hills AP5155-HA Polypropylene Impact Copolymer Features: Excellent processability, nucleated and Antistat.Applications: Injection molding: thin wall parts, food containers, packaging and medicalInformation Provided by Flint Hills Resources |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla.. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature 23.0 °C |
1.11 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -30.0 °C |
1.11 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -30.0 °C |
1.11 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -40.0 °C |
1.11 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 264-15 PPO, 15% Glass Reinforced A general purpose, 15% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 520S-13GU Nylon 66, 13% Glass Reinforced Nylon 66, 13% Glass reinforced resin with heat stabilizer, utility grade. Also available in black (520S-13GBU).Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | Wet; ASTM D256 |
Asahi Kasei Leona® 14G15 15% Glass Filled Nylon 66 15% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Heater tanks, fuel injectors, ABS sensors, and other under-the-hood automotive parts Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 747 Nylon 6/66 A medium viscosity copolymer. Excellent flexibility and elongation suitable for film and monofilament applications.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 1132P Cellulose Reinforced Phenolic Novolac FM 1132P is a two-stage phenolic molding compound reinforced with cellulose in pellet form. FM-1132P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-10. (Replaces Militar.. |
|||
Izod Impact, Notched | 0.590 J/cm @Diameter 3.17 mm |
1.11 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Accpro® 9117 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Sheet; ExtrusionFeatures: Improved MVTR, Stain resistanceTypical applications: Film, Rigid packagingComplies with FDA specification, Title 21, CFR 177.1520.Typical pro.. |