Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D412 |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature -30.0 °C |
1.09 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp OFP36A PPS - Branched (Asia Pacific) LNP LUBRICOMP* OFP36A is a compound based on PPS - Branched resin containing Silicone, PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.This data was supplied by SA.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT LNP* Lubricomp* WX95752L is a compound based on Polybutylene Terephalate resin. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT (Asia Pacific) LNP* Lubricomp* WX95752L is a compound based on Polybutylene Terephalate resin. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS LNP* THERMOCOMP* AF006XXZ is a compound based on ABS resin containing 30% Glass Fiber. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX05475 PC LNP* THERMOCOMP* DX05474 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing 20% Milled Glass. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU (Asia Pacific) LNP* THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 LNP* THERMOCOMP* RF0079SZ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP XFL21R PA LNP* LUBRICOMP* XFL21R is a compound based on Amorphous Nylon resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Mold Release. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct.. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature -30.0 °C |
1.09 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC LNP* THERMOCOMP* DC0049XF is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX2926 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX2926 compound is a reinforced high modulus PPE+PS. 5VA rated at 2.5 in black and at 3.0 in gray. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF004S PA 6 (Asia Pacific) LNP* Thermocomp* PF004S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P106 PBT Polyester A general purpose polyester with low shrinkage and good flow.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL CN5260 PPE+PS (Asia Pacific) 50% filled FR high modulus PPE/PS blend |