Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.530 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ AT-000/05T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded, Across Flow; ASTM D256A |
PolyOne Nymax™ 1200 A Zip 22 Natural Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Nylene® PA6 Homopolymer 201 Nylon 6; Low Viscosity Nucleated Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Plenco 50015 PET, Pellet, Injection Molded Natural Color
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature -40.0 °C |
0.993 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Rotuba H5 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature -30.0 °C |
0.993 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.17 mm |
0.993 ft-lb/in @Thickness 0.125 in |
|
KEP Kepital® F20-52 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Global PBT-325 Polybutylene Terephthalate Alloy Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 215HPR PBT Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC (Asia Pacific) LNP* Stat-kon* DE0069F is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, , Flame Retardant. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+PS LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific) LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 (Asia Pacific) LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3452 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3452 is a 30% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 584 mm |
0.993 ft-lb/in @Thickness 23.0 in |
ISO 180/A |
BASF Ultraform N 2310P Q600 POM Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 164 Polypropylene, Mineral Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | Conditioned; ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer b.. |