Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.490332 - 980.567 J/cm @Temperature -40.0 - -40.0 °C |
0.918594 - 1837.00 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.16 J/cm Grade Count:27 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.490332 - 980.567 J/cm @Thickness 6.40 - 6.40 mm |
0.918594 - 1837.00 ft-lb/in @Thickness 0.252 - 0.252 in |
Average value: 1.16 J/cm Grade Count:27 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.490332 - 0.490332 J/cm @Temperature 3.20 - 3.20 °C |
0.918594 - 0.918594 ft-lb/in @Temperature 37.8 - 37.8 °F |
Average value: 0.427 J/cm Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.490332 - 0.490332 J/cm @Thickness 23.0 - 23.0 mm |
0.918594 - 0.918594 ft-lb/in @Thickness 0.906 - 0.906 in |
Average value: 0.427 J/cm Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.490332 - 3.43233 J/cm @Temperature -20.0 - 0.000 °C |
0.918594 - 6.43016 ft-lb/in @Temperature -4.00 - 32.0 °F |
Average value: 1.91 J/cm Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.490332 - 980.567 J/cm @Temperature -40.0 - -40.0 °C |
0.918594 - 1837.00 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.22 J/cm Grade Count:16 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.490332 - 980.567 J/cm @Thickness 3.17 - 3.17 mm |
0.918594 - 1837.00 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.22 J/cm Grade Count:16 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |