Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.17 mm |
0.899 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® X AS-40CF/000 Natural SE Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 6.35 mm |
0.899 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.480 - 4.00 J/cm @Thickness 3.17 - 6.40 mm |
0.899 - 7.49 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 1.28 J/cm Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2212 PEI (Asia Pacific) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -30.0 °C |
0.899 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX99620C PC LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10 LNP* THERMOCOMP* QF004 is a compound based on Nylon 6/10 resin containing 20% Glass Fiber. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WH0500B PBT LNP* THERMOCOMP* WH0500B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was .. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Bapolene® 3262 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This resin offers intermediate flow, excellent ESCR, excellent impact and good warp resistance. This product meets FDA standards for f.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 612 Nylon 6, Glass Fiber/Bead Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
(discontinued **) Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still.. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 6.35 mm |
0.899 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® ES-06CF-09GF/000 RED Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications
& Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific) LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2110N PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |