Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | ASTM D256 |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.827 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG.. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.827 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCON CP6052 PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi.. |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.827 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3302 PP+MF30% Description: Injection Molding, PP+MF30%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | DIN 53453; ASTM D256 |
Kolon NOPLA® KE931 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.827 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2156FL PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by.. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.827 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HV1005S PBT Description: Injection Molding, PBT, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.827 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® LW5102F PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information.. |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.35 mm |
>= 0.827 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.35 mm |
>= 0.827 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.35 mm |
>= 0.827 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1100-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.827 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HM3207SM PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, Good Weatherability, High ImpactApplication: Automotive Interior Parts CAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.441 J/cm @Temperature 23.0 °C |
0.827 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 1196NN Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER UNREINFORCED, CONTAIN FLAME RETARDANT, UL 94 V-2 APPROVAL, HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES |
|||
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | |
Shinil Chemical SHINSTRA PP (SM400) Structural Polymer Household SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.17 mm |
0.827 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TN-1200 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.17 mm |
0.827 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XK-2307 PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.17 mm |
0.827 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TN-1200 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.441 J/cm @Thickness 3.17 mm |
0.827 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XK-2307 PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | |
Zylog Hipolyene® 8021 M Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6C1 Nylon 6, 10% Mineral Reinforced |
|||
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6CV1 Flame Retardant Nylon 6, 10% Mineral Reinforced |
|||
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB120CR Fast Crystallinity PA6 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Izod Impact, Notched | 0.441 J/cm @Temperature 23.0 °C |
0.827 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
Beijing Ranger Chem BLUESTAR® BS450 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Notched | 0.441 J/cm | 0.827 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FRCV100 Flame Retardant Nylon 66, 10% Mineral Reinforced |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.35 mm |
>= 0.827 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1100-211MB Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.35 mm |
>= 0.827 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 3015-104 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Izod Impact, Notched | >= 0.441 J/cm @Thickness 6.35 mm |
>= 0.827 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |