Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.42712 - 7.68816 J/cm @Temperature -40.0 - -18.0 °C |
0.80017 - 14.4031 ft-lb/in @Temperature -40.0 - -0.400 °F |
Average value: 1.66 J/cm Grade Count:31 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 0.42712 - 0.800 J/cm @Temperature -17.8 - 0.000 °C |
0.80017 - 1.50 ft-lb/in @Temperature 0.000 - 32.0 °F |
Average value: 0.614 J/cm Grade Count:2 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.42712 - 0.58729 J/cm @Temperature 0.000 - 0.000 °C |
0.80017 - 1.1002 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.534 J/cm Grade Count:3 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |
|||
Izod Impact, Notched | 0.42712 - 0.58729 J/cm @Diameter 6.35 - 6.35 mm |
0.80017 - 1.1002 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.534 J/cm Grade Count:3 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |